Name | acrylonitrile fiber oiling agent 101 |
Synonyms | Nitrile oil 101 |
Physical and Chemical Properties | Chemical properties light yellow to yellow oily liquid, which can be diluted with water in arbitrary proportions. Good heat resistance, stable emulsion, low oil consumption, stable fiber oil content, high oil film strength, good looseness, and can prevent wire merging under strong crimping conditions. |
Use | Use of textile oil agent, suitable for dry roll oil acrylic process of cotton fiber oil. Can make the fiber feel soft and smooth, improve spinnability and weaving. |
Store in a cool and shaded area, away from sources of ignition. Protect from sunlight and rain during transportation.
Mix 25 parts of fatty acid polyethylene glycol ester, 7 parts of polyether, 20 parts of alkyl polyoxyethylene ether, 10 parts of polyoxyethylene stearate, 30 parts of alkyl phosphate ammonium salt, and 10 parts of alkyl alcohol amide evenly, heat and dissolve them, and add water under stirring until the effective content is about 50%. It is best to stir at 60-70 ℃ for 0.5h to generate a light yellow transparent liquid. Cooling and discharging, packaging to obtain the finished product.
25 parts of fatty acid polyethylene glycol ester, 7 parts of polyether, 20 parts of alkyl polyoxyethylene ether, 10 parts of polyoxyethylene stearate, 30 parts of alkyl phosphate ammonium salt and 10 parts of alkyl alcohol amide are mixed evenly, heated and dissolved, and water is added under stirring until the effective substance content is about 50%. It is best to stir at 60~70 ℃ for 0.5 h to generate light yellow transparent liquid. Cooling and discharging, packaging can be finished.